S690QL1 steel plate

Oct 13, 2025 Остави съобщение

S690QL1 is a quenched and tempered, high-strength structural steel plate that conforms to the EN 10025-6 standard. It has a minimum yield strength of 690 MPa and is designed for low-temperature impact performance down to −60 ℃. This steel is used for manufacturing structural components in construction, mining, and other industries requiring high strength and toughness, such as cranes, excavators, and loading machines.

 

EN10025-6 S690QL1

THK: 3 to 300, Width: 1500 to 4050, Length: 3000 to 27000

 

 

S690QL1

 

S690QL1 

C

P

S

N

B

S690 QL1

0.20

0.80

1.70

0.020-0.025

0.010-0.015

0.015

0.005

1.50

V

 

0.50

0.70

0.06

2.0

0.05

0.12

0.15

 

Carbon Equivalent: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

 

S690QL1 

 

S690QL1

 

S690 QL1

-60

30J

3<>

890

940-1100

11

-60

30J

50<>

830

880-1100

11

-60

30J

100<>

800

820-1000

11

-60

30J